Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1150 - 1400 cP @Temperature 23.0 °C |
1150 - 1400 cP @Temperature 73.4 °F |
|
Prodways PLASTCure Model 100 3D Printing Polymer Allows production of precise components; high workability.Used for dental applications from models for restorations to orthodontics.Information provided by Genistar. |
|||
Viscosity | 1000 - 1400 cP @Temperature 25.0 °C |
1000 - 1400 cP @Temperature 77.0 °F |
|
Northstar Polymers PND-011 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 800 - 1400 cP @Temperature 71.1 °C |
800 - 1400 cP @Temperature 160 °F |
|
Northstar Polymers SBX-146 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 1200 - 1400 cP @Temperature 25.0 °C |
1200 - 1400 cP @Temperature 77.0 °F |
|
Northstar Polymers MPC-038 MDI Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 1000 - 1400 cP @Temperature 25.0 °C |
1000 - 1400 cP @Temperature 77.0 °F |
|
Northstar Polymers MPG-023 Isocyanate Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1184 A (SBS) Branched Block Copolymer Description: Kraton D1184 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1184 E (SBS) Branched Block Copolymer Description: Kraton D1184 E is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 15% Toluene Solution at 25°C; KM 06 |
Kraton® D1186 A (SBS) Branched Block Copolymer Description: Kraton D1186 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 15% Toluene Solution at 25°C; KM 06 |
Kraton® D1186 B (SBS) Branched Triblock Copolymer Description: Kraton D1186 BT is a clear, branched triblock copolymer based on styrene and butadiene with a polystyrene content of 30%. It is supplied from South America in the physical form identifi.. |
|||
Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 15% Toluene Solution at 25°C; KM 06 |
Kraton® D1186 E (SBS) Branched Block Copolymer Description: Kraton D1186 E is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-737 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Non-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for.. |
|||
Viscosity | 1200 - 1400 cP | 1200 - 1400 cP | mixed compound |
Master Bond EP30P Epoxy Bonds Glass, Polycarbonates and Acrylics Description: Master Bond Polymer Adhesive EP30P is a two component, transparent, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is for.. |
|||
Viscosity | 110 - 1400 cP | 110 - 1400 cP | |
Beijing Ranger Chem E-52D Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 900 - 1400 cP | 900 - 1400 cP | #3 SP @ 60 rpm; RP-0596 |
Solvay RHODOLINE® 640 Surfactant Description: Mineral oil based defoamers for flat to gloss paints, great process foam know down.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© 640 is a hydroph.. |