Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 140 - 40000 cP @Temperature 121 - 190 °C |
140 - 40000 cP @Temperature 250 - 374 °F |
Average value: 495000 cP Grade Count:42 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Viscosity | 140 cP @Temperature 121 °C |
140 cP @Temperature 250 °F |
melt viscosity; ASTM D-3236 |
ExxonMobil Escorene® MV 02514 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 14% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Viscosity | 140 cP | 140 cP | |
KKPC KOSYN KSL 103 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 100 series are carboxy metamorphic styrene-butadiene latexes. They have a soft touch and high adhesive force.Applications: Carpet Backing, Adhesive .. |
|||
Viscosity | 140 cP | 140 cP | |
BASF Lupranate® 223 Isocyanate Description: Lupranate® 223 Isocyanate is a low viscosity derivative of both pure-MDI and polymeric-MDI. With a functionality of approximately 2.2, this isocyanate can be formulated into applicatio.. |
|||
Viscosity | 140 cP | 140 cP | |
BASF Lupranate® 5040 Isocyanate Description: Lupranate® 5040 Isocyanate has the combined characteristics of a liquid carbodiimidemodified isocyanate and a pure MDI prepolymer. The relatively low functionality and high free-NCO of.. |
|||
Viscosity | 140 cP | 140 cP | at 20% solids (MEK/Ethyl acetate 50/50 by wt) |
DuPont Performance Polymers Hypalon® CP-337 Adhesion Primer, General Description
(discontinued **) Hypalon CP 337 is a chlorinated, medium viscosity, ethylene (meth) acrylic acid copolymer. This unique resin has been developed to improve adhesion to ethylene vinyl acetate copolymers. Hypalon CP 3.. |
|||
Viscosity | 140 - 220 cP | 140 - 220 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® G1726 M (SEBS) Linear Triblock Copolymer Description: Kraton G1726 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |