Polymer Property : Viscosity = 12400 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 12400 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
12400 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O..
Viscosity 12400 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
12400 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-55-1000 TPE
Product Description: StarXTRUDE XTR-55-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P..
Viscosity 12400 cP
12400 cP
mixing, dynamic
Dow Corning SILASTIC® 3498 MOULD MAKING BASE & 96 CURING AGENT
High strength, low hardness, fast cure silicone mold making rubber featuring a very good resistance to polyester resin and suited for the detailed reproduction of fiines, art objects and similar ite..