Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 11200 cP | 11200 cP | mixing, dynamic |
Dow Corning SILASTIC® 3496 MOULD MAKING BASE & 96 CURING AGENT High strength, low hardness, fast cure silicone mold making rubber featuring a very good resistance to polyester resin and suited for the detailed reproduction of fiines, art objects and similar ite.. |
|||
Viscosity | 11200 cP @Temperature 177 °C |
11200 cP @Temperature 350 °F |
Typical |
Bostik 130 General Purpose EVA Glue Stick Bostik 130 General Purpose EVA Glue StickGeneral purpose for a variety of substrates including ABS in general assembly. |