Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 102000 cP | 102000 cP | |
Dow Corning SE 4448 CV KIT PARTS A&B Excellent thermal conductivity, low volatility (D4-D10 0.03% wt), heat cure, high viscosity.Information provided by Dow Corning |
|||
Viscosity | 102000 cP @Shear Rate 300 1/s, Temperature 190 °C |
102000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NCEHT Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040NCEHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with
improved surface.. |