Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.75e+6 - 2.05e+6 cP | 1.75e+6 - 2.05e+6 cP | Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF) Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanical.. |
|||
Viscosity | 1.75e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
1.75e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F136 PA6 Very High Viscosity, Film Extrusion |
|||
Viscosity | 1.75e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
1.75e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F136-C PA6 Film Extrusion, Very High Viscosity, Lubricated |
|||
Viscosity | 1.75e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
1.75e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F136-C1 PA6 Very High Viscosity, Film Extrusion, Lubricated |
|||
Viscosity | 1.75e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
1.75e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F136-E1 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Viscosity | 1.75e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
1.75e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F136-E2 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |