Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 1.20e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1.20e+6 cP
1.20e+6 cP
Part B, RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP1121-4 Adhesive / Casting Resin
Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives ..
Viscosity 1.20e+6 cP
1.20e+6 cP
Melt Viscosity; SABIC Method
SABIC Innovative Plastics Valox® 337 PBT
Low temperature impact PBT. Automotive applications: underhood power distribution boxes and covers.
Viscosity 1.20e+6 cP
1.20e+6 cP
A
Shin-Etsu Silicones LIMSâ„¢ KEG2000-70A/B Elastomer
KEG2000-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
Viscosity 1.20e+6 cP
1.20e+6 cP
B
Shin-Etsu Silicones LIMSâ„¢ KEG2000-70A/B Elastomer
KEG2000-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
Viscosity 1.20e+6 cP
1.20e+6 cP
B
Shin-Etsu Silicones LIMSâ„¢ KEG2001-40A/B Elastomer
KEG2001-40 is a very fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enou..
Viscosity 1.20e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
1.20e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Viscosity 1.20e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
1.20e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 3861 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Viscosity 1.20e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
1.20e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 3930 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Viscosity 1.20e+6 cP

@Temperature 160 °C
1.20e+6 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® D 1519E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 1.20e+6 cP

@Load 5.00 kg,
Temperature 250 °C
1.20e+6 cP

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Diamond Polymers NPP 60-1300 GF30 30% Glass Filled Polyester Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Viscosity 1.20e+6 cP
1.20e+6 cP
3M Scotch-Weld™ DP604NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesive DP-604NS is a black, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in a duo-pak cartridge. With the squeeze of the trigger, the ..
Viscosity 1.20e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.20e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® 2821-00 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi..
Viscosity 1.20e+6 - 1.80e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.20e+6 - 1.80e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® EXAD 3000 Polyvinylidene Fluoride - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Extrusion aid, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanic..
Viscosity 1.20e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.20e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Copyright © lookpolymers.com All Rights Reserved