Polymer Property : Viscosity = 1.12e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1.12e+6 cP

@Temperature 260 °C
1.12e+6 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F132 PA6
Film Extrusion, High Viscosity
Viscosity 1.12e+6 cP

@Temperature 260 °C
1.12e+6 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
Viscosity 1.12e+6 cP

@Temperature 260 °C
1.12e+6 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F132-E1 PA6
Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion
Viscosity 1.12e+6 cP

@Temperature 260 °C
1.12e+6 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F132-E2 PA6
High Viscosity, Nucleated, Lubricated, Film Extrusion