Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.1 cP @Temperature 25.0 °C |
1.1 cP @Temperature 77.0 °F |
|
LyondellBasell Ethanol, 200 Proof Information provided by Lyondell. |
|||
Viscosity | 1.1 cP @Temperature 25.0 °C |
1.1 cP @Temperature 77.0 °F |
|
LyondellBasell PMA Propylene glycol methyl ether acetate Available in electronic grade.Information provided by Lyondell. |
|||
Viscosity | 1.1 cP @Temperature 25.0 °C |
1.1 cP @Temperature 77.0 °F |
|
LyondellBasell PMP Propylene glycol methyl ether propionate Information provided by Lyondell. |
|||
Viscosity | 1.1 cP | 1.1 cP | Inherent; ASTM D1243 |
Formosa Plastics Formolon® 45 PVC PVC Copolymer Dispersion Resin F-45 is a vinyl chloride vinyl acetate copolymer dispersion resin with low paste viscosities, excellent heat stability, and rapid fusion characteristics. F-45 has been.. |