Physical Properties Metric English Comments
Melt Index of Compound 2.0 - 9.0 g/10 min

@Temperature 190 °C
2.0 - 9.0 g/10 min

@Temperature 374 °F
P=49, 1 H
Sibur DST-45 RM Styrene-Butadiene-Styrene Block Copolymer (SBS-TPE)
Kraton D 4271. For production of footwear compositions.
Melt Index of Compound 7.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Arkema Group LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 20 MA 08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MA 08 is a polyme..
Melt Index of Compound 7.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Arkema Group OREVAC® 18722 Maleic Anhydride Modified Polypropylene
OREVAC 18722 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18722 ..
Melt Index of Compound 7.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Arkema Group LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4603 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure process in autoclave reactor. LOTADER 4603 is a multipurpose extrusion adhesive used..
Melt Index of Compound 7.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Arkema Group LOTRYL® 20 MBG 08 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 20MBG08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MBG 08 is a polyme..