Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 6.5 - 8.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.5 - 8.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTRYL® 17 BA 07 Copolymer Ethylene - Butyl Acrylate LOTRYL® 17 BA 07 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 17 BA 07 is used as tie layer in coextrusion PP/PE, for extrusi.. |