Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 60 g/10 min @Load 2.16 kg, Temperature 190 °C |
60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Melt Index of Compound | 60 g/10 min @Load 2.16 kg, Temperature 190 °C |
60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Melt Index of Compound | 60 g/10 min @Load 10.0 kg, Temperature 190 °C |
60 g/10 min @Load 22.0 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a.. |
|||
Melt Index of Compound | 60 g/10 min @Load 10.0 kg, Temperature 190 °C |
60 g/10 min @Load 22.0 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe.. |
|||
Melt Index of Compound | 60 g/10 min @Load 10.0 kg, Temperature 210 °C |
60 g/10 min @Load 22.0 lb, Temperature 410 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester Introduction: IROGRAN A 94 E 4900 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe.. |
|||
Melt Index of Compound | 60 g/10 min @Load 5.00 kg, Temperature 190 °C |
60 g/10 min @Load 11.0 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® CA116-205 TPU-Polyester Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and shee.. |
|||
Melt Index of Compound | 60 g/10 min @Load 2.16 kg, Temperature 190 °C |
60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |