Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 50.85 g/10 min @Load 10.0 kg, Temperature 220 °C |
50.85 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
LG Chemical AF-348 ABS, Flame Retardant, Heat Resistant, Weather Resistant Information Provided by LG Chem |