Physical Properties Metric English Comments
Melt Index of Compound 5.8 - 7.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.8 - 7.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating
The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a..
Melt Index of Compound 5.8 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.8 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
LG Chemical IG840 PMMA, General Purpose Grade for Injection Molding
General purpose grade with better flowability than IH 830 but slightly below in heat resistanceMechanical strength and surface hardnessFeatures: Excellent transparency and eleganceWeather resistance..