Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 5.775 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.775 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
LG Chemical RS-800 ABS, Extrusion, High Impact, HCFC Resistant Information Provided by LG Chem |