Polymer Property : Melt Index of Compound = 5.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 2.5 - 5.5 g/10 min
2.5 - 5.5 g/10 min
Sibur ABS 0809 Molding Grade ABS Plastic
With high thermal stability and rigidity for small automobile products and working under higher temperatures.