Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 35 - 45 g/10 min @Load 2.16 kg, Temperature 190 °C |
35 - 45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTRYL® 35 BA 40 Copolymer Ethylene - Butyl Acrylate LOTRYL® 35 BA 40 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 35% in weight. LOTRYL® 35 BA 40 is particularly r.. |
|||
Melt Index of Compound | 35 - 45 g/10 min @Load 2.16 kg, Temperature 190 °C |
35 - 45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 28-40 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-40 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-40 is stabilized with antioxidants. The High Vinyl Acetate co.. |