Physical Properties Metric English Comments
Melt Index of Compound 43 g/10 min

@Load 2.16 kg,
Temperature 330 °C
43 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer
FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C.
Melt Index of Compound 43 g/10 min

@Load 1.20 kg,
Temperature 300 °C
43 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
Melt Index of Compound 43 g/10 min

@Load 1.20 kg,
Temperature 300 °C
43 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
Melt Index of Compound 43 g/10 min

@Load 1.20 kg,
Temperature 300 °C
43 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East)
Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm.
Melt Index of Compound 43 g/10 min

@Load 2.16 kg,
Temperature 330 °C
43 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Melt Index of Compound 43 g/10 min

@Load 2.16 kg,
Temperature 330 °C
43 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Melt Index of Compound 43 g/10 min

@Load 2.16 kg,
Temperature 330 °C
43 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Melt Index of Compound 43 g/10 min

@Load 2.16 kg,
Temperature 330 °C
43 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East)
XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors.
Melt Index of Compound 43 g/10 min

@Load 2.16 kg,
Temperature 330 °C
43 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Melt Index of Compound 43 g/10 min

@Load 2.16 kg,
Temperature 330 °C
43 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East)
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Melt Index of Compound 43 g/10 min

@Load 1.20 kg,
Temperature 300 °C
43 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific)
Transparent Polycarbonate in natural color. Excellent processability, super high flow.
Melt Index of Compound 43 g/10 min

@Load 2.16 kg,
Temperature 330 °C
43 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific)
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..