Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 32 - 37 g/10 min @Load 2.16 kg, Temperature 190 °C |
32 - 37 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTRYL® 35 BA 320 Copolymer Ethylene - Butyl Acrylate LOTRYL® 35 BA 320 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 35% in weight. LOTRYL® 35 BA 320 is particularly.. |