Polymer Property : Melt Index of Compound = 33 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific)
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Asia Pacific)
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® HPXS8R PC Copolymer
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Melt Index of Compound 33 g/10 min

@Load 10.0 kg,
Temperature 210 °C
33 g/10 min

@Load 22.0 lb,
Temperature 410 °F
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester
Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN ..
Melt Index of Compound 33 g/10 min

@Load 5.00 kg,
Temperature 280 °C
33 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® V9561 PET
Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances.
Melt Index of Compound 33 g/10 min

@Load 2.16 kg,
Temperature 190 °C
33 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Melt Index of Compound 33 g/10 min

@Load 2.16 kg,
Temperature 190 °C
33 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Melt Index of Compound 33 g/10 min

@Load 2.16 kg,
Temperature 190 °C
33 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Melt Index of Compound 33 g/10 min

@Load 2.16 kg,
Temperature 190 °C
33 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Melt Index of Compound 33 g/10 min

@Load 2.16 kg,
Temperature 190 °C
33 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Melt Index of Compound 33 g/10 min
33 g/10 min
ASTM D1238
Cheng Yu Plastic 3276 TPE Rubber
Melt Index of Compound 33 g/10 min

@Load 2.16 kg,
Temperature 190 °C
33 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Melt Index of Compound 33 g/10 min

@Load 5.00 kg,
Temperature 280 °C
33 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East)
Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances.