Melt Index of Compound 32 g/10 min

@Load 2.16 kg,
Temperature 250 °C
32 g/10 min

@Load 4.76 lb,
Temperature 482 °F
cm3/10 min; ISO 1133
DuPont Performance Polymers Crastin® S600F40 NC010 PBT  (Unverified Data**)
Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Melt Index of Compound 32 g/10 min

@Load 5.00 kg,
Temperature 300 °C
32 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific)
Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade.
Melt Index of Compound 32 g/10 min

@Load 5.00 kg,
Temperature 280 °C
32 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS
EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l..
Melt Index of Compound 32 - 37 g/10 min

@Load 2.16 kg,
Temperature 190 °C
32 - 37 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Arkema Group LOTRYL® 35 BA 320 Copolymer Ethylene - Butyl Acrylate
LOTRYL® 35 BA 320 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 35% in weight. LOTRYL® 35 BA 320 is particularly..
Melt Index of Compound 32 g/10 min

@Load 10.0 kg,
Temperature 280 °C
32 g/10 min

@Load 22.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has ..