Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 21 - 25 g/10 min | 21 - 25 g/10 min | |
Sibur 21230 Polypropylene Compounding for stabilization 16K, 16V, 16N, 16M, 16H superior quality. For production of technical and domestic products of complicated profile, of non-woven materials. |
|||
Melt Index of Compound | 8.0 - 25 g/10 min | 8.0 - 25 g/10 min | ASTM D1238, ISO 1133 |
EPICHEM Epicarb PC BLACK IQ Polycarbonate Characteristics: good fluidity, good impact, industrial quality |
|||
Melt Index of Compound | 15 - 25 g/10 min @Load 5.00 kg, Temperature 265 °C |
15 - 25 g/10 min @Load 11.0 lb, Temperature 509 °F |
|
3M Dyneon™ FX 5912 Dynamar™ Polymer Processing Additive Dynamar FX 5912 is a free-flowing fluorothermoplastic processing aid that is designed for use at very low levels to improve the processing of thermoplastics. Typical use levels of 200 to 1000 ppm ha.. |
|||
Melt Index of Compound | 10 - 25 g/10 min @Temperature 125 °C |
10 - 25 g/10 min @Temperature 257 °F |
MA109RPL |
C.O.I.M. FILCO® 661 FPG 005 Powder Binder for Glass Mat Description: Powder Binder for Glass MatGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are coll.. |