Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 260 °C |
21 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Asia Pacific) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 260 °C |
21 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY4000 PC+ABS (Europe-Africa-Middle East) Cycoloy* CY4000 resin is an injection moldable, flame retardant PC/ABS blend free of brominated or chlorinated flame resistant additives. Cycoloy CY4000 has excellent flow and balanced impact proper.. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 223R PC (Europe-Africa-Middle East) LEXAN 223R is a low viscosity, UV stabilized multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 915AU PC (Europe-Africa-Middle East) LEXAN resin grade 915AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in transparent colors, inte.. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 920 PC (Europe-Africa-Middle East) LEXAN 920 is a low viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 923 PC (Europe-Africa-Middle East) LEXAN 923 is a low viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXD121R PC (Europe-Africa-Middle East) LEXAN FXD121R is a transparent/translucent low viscosity grade for light diffusion special effects. Color package may affect performance. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXD123R PC (Europe-Africa-Middle East) LEXAN FXD123R is a transparent/translucent low viscosity grade for light diffusion special effects. UV-stabilized. Color package may affect performance. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM121R PC (Europe-Africa-Middle East) LEXAN FXM121R is a transparent/translucent low viscosity grade for special effects colors with a metallic-luster appearance. Color package may affect performance. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM123R PC (Asia Pacific) FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package .. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP2EU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol.. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® IR1840 PC (Europe-Africa-Middle East) IR1840 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® LI1911R PC (Europe-Africa-Middle East) Low-viscosity multi-purpose grade having low levels of ionics species. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® LS1 PC (Europe-Africa-Middle East) LEXAN LS1 is a low viscosity injection moulding grade especially designed for manufacturing complex parts requiring easy flow properties combined with high optical requirements. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific) Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame.. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® PC2200 PC (Europe-Africa-Middle East) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 190 °C |
21 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics PC2203R PC (Europe-Africa-Middle East) PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 265 °C |
21 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 265 °C |
21 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Melt Index of Compound | 21 - 25 g/10 min | 21 - 25 g/10 min | |
Sibur 21230 Polypropylene Compounding for stabilization 16K, 16V, 16N, 16M, 16H superior quality. For production of technical and domestic products of complicated profile, of non-woven materials. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 280 °C |
21 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Melt Index of Compound | 21 g/10 min @Load 5.00 kg, Temperature 300 °C |
21 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Melt Index of Compound | 21 g/10 min @Load 5.00 kg, Temperature 300 °C |
21 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Asia Pacific) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 250 °C |
21 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific) Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications. |