Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.8 - 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 - 2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TS 9022 MDPE - Overwrap Packaging The Trithene TS 9022 resin is a medium-density polyethylene (MDPE) with good optical properties, excellent stiffness and processability, that warrants the production of thin films with good appearan.. |
|||
Melt Index of Compound | 1.8 - 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 - 2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing .. |
|||
Melt Index of Compound | 1.8 - 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 - 2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar.. |