Polymer Property : Melt Index of Compound = 19.76 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 19.76 g/10 min

@Load 10.0 kg,
Temperature 220 °C
19.76 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
LG Chemical HI-121 ABS, High Impact
Feature: Injection Molding, Well Balanced Mechanical PropertiesApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information Provided by LG Chem