Polymer Property : Melt Index of Compound = 19 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 19 g/10 min

@Load 2.16 kg,
Temperature 260 °C
19 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Melt Index of Compound 19 g/10 min

@Load 2.16 kg,
Temperature 260 °C
19 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Melt Index of Compound 19 g/10 min

@Load 5.00 kg,
Temperature 260 °C
19 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CY8540 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CY8540 is a PC+ABS blend, especially designed for textile backmolding in automotive interior applications. High flow grade, which allows low temperature processing to maintain fabric integri..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer
Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Asia Pacific)
Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer
Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific)
Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer
Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific)
Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer
Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer
Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Asia Pacific)
Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch..
Melt Index of Compound 19 g/10 min

@Load 3.80 kg,
Temperature 300 °C
19 g/10 min

@Load 8.38 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics LNP STAT-KON DEL32P PC (Asia Pacific)
LNP* Stat-kon* DEL32P is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive.
Melt Index of Compound 19 g/10 min

@Load 2.16 kg,
Temperature 300 °C
19 g/10 min

@Load 4.76 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics LNP STAT-KON DX13320C PC COPOLYMER (Asia Pacific)
LNP* Statkon DX13320C is ultra clean polycarbonate/carbon fiber compound with high modulus, good flow ability, easy mold release, and high level of cleanliness for the most demanding application. A ..
Melt Index of Compound 19 g/10 min

@Load 2.16 kg,
Temperature 250 °C
19 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® HX3091HP PBT
PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only.
Melt Index of Compound 19 g/10 min

@Load 5.00 kg,
Temperature 280 °C
19 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Melt Index of Compound 19 g/10 min

@Load 5.00 kg,
Temperature 280 °C
19 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific)
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Melt Index of Compound 19 g/10 min

@Load 5.00 kg,
Temperature 280 °C
19 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East)
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Melt Index of Compound 19 g/10 min

@Load 10.0 kg,
Temperature 280 °C
19 g/10 min

@Load 22.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East)
NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306.
Melt Index of Compound 19 g/10 min

@Load 2.16 kg,
Temperature 260 °C
19 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Melt Index of Compound 19 g/10 min

@Load 1.20 kg,
Temperature 224 °C
19 g/10 min

@Load 2.65 lb,
Temperature 435 °F
ASTM D1238
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **)
Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C..