Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Index of Compound = 155 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 155 g/10 min

@Load 2.16 kg,
Temperature 190 °C
155 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ICO Polymers ICOFLOâ„¢ 510-5023 400 Micron LDPE Powder
Description: ICOFLO 510-5023 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Melt Index of Compound 155 g/10 min

@Load 2.16 kg,
Temperature 190 °C
155 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder
Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Melt Index of Compound 155 g/10 min

@Load 2.16 kg,
Temperature 190 °C
155 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ICO Polymers ICOFLOâ„¢ 510-5063 800 Micron LDPE Powder
Description: ICOFLO 510-5063 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Melt Index of Compound 155 g/10 min

@Load 2.16 kg,
Temperature 190 °C
155 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ICO Polymers ICOTEXâ„¢ 520-5062 500 Micron LDPE Powder
Description: ICOTEX 520-5062 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, ..
Melt Index of Compound 155 g/10 min

@Load 2.16 kg,
Temperature 190 °C
155 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ICO Polymers ICOFLOâ„¢ 510-5064 1200 Micron LDPE Powder
Description: ICOFLO 510-5064 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Melt Index of Compound 155 g/10 min

@Load 2.16 kg,
Temperature 190 °C
155 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow
Copyright © lookpolymers.com All Rights Reserved