Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE EC90 D50 P05B Thermoplastic Elastomer, PP/EPDM Information provided by Polykemi AB |
|||
Melt Index of Compound | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXD143R PC (Europe-Africa-Middle East) LEXAN FXD143R is a transparent/translucent medium viscosity grade for light diffusion effects. UV-stabilized. The color package may affect performance. |
|||
Melt Index of Compound | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE141R PC (Europe-Africa-Middle East) LEXAN FXE141R is a medium viscosity multi purpose UV stabilized grade for visual effects in ""energy"". The material contains a release agent to ensure easy processing. |
|||
Melt Index of Compound | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Melt Index of Compound | 11 g/10 min @Load 1.20 kg, Temperature 250 °C |
11 g/10 min @Load 2.65 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML7687 PC (Europe-Africa-Middle East) ML7687 is an optical quality, high purity PC resin optimized for use in optical applications such as light guide panels |
|||
Melt Index of Compound | 11 g/10 min @Load 1.20 kg, Temperature 250 °C |
11 g/10 min @Load 2.65 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® OQ1026 PC (Asia Pacific) LEXAN OQ1026 is an optical quality, high purity PC resin optimized for the demanding short cycle times used in DVD production. Advances in technology further enhanced the processability while mainta.. |
|||
Melt Index of Compound | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM141R PC (Asia Pacific) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 360 °C |
11 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 360 °C |
11 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 300 °C |
11 g/10 min @Load 4.76 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP EXTC8141 PC (Asia Pacific) LNP* Thermocomp* EXTC8141 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No.. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 300 °C |
11 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP ZX08309 PPE+HIPS (Asia Pacific) This material is mineral filled PPO grade with high dielectric constant and low loss tangent |
|||
Melt Index of Compound | 11 g/10 min @Load 10.0 kg, Temperature 300 °C |
11 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 220 °C |
11 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM HU2410 PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Melt Index of Compound | 11 - 15 g/10 min @Load 2.16 kg, Temperature 250 °C |
11 - 15 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Shinkong Synthetic Fibers Shinite® D201K011 PBT, Super Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Melt Index of Compound | 11 g/10 min @Load 10.0 kg, Temperature 280 °C |
11 g/10 min @Load 22.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East) Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating .. |
|||
Melt Index of Compound | 11 g/10 min @Load 10.0 kg, Temperature 300 °C |
11 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Melt Index of Compound | 11 g/10 min @Load 8.70 kg, Temperature 190 °C |
11 g/10 min @Load 19.2 lb, Temperature 374 °F |
ASTM D1238 |
Advanced Polymer Alloys DuraGrip™ 6165 TR Thermoplastic Elastomer DuraGrip® DGR6165TR is a translucent thermoplastic elastomer (TPE) formulated for excellent elastic properties and enhanced adhesion to engineered thermoplastics using insert molding, co-injection .. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Melt Index of Compound | 11 g/10 min | 11 g/10 min | Q-409A-87 (JIS K 7210) |
Zeon Chemicals Quintac® 3280 SIS Rubber |
|||
Melt Index of Compound | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML3260 PC (Europe-Africa-Middle East) LEXAN ML3260 is a medium viscosity, 15% glass reinforced, flame retardant grade especially designed for applications like computer cartridges. |