Polymer Property : Melt Index of Compound = 1.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 1.0 - 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 - 1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Arkema Group LOTRYL® 7 BA 01 Copolymer Ethylene - Butyl Acrylate
LOTRYL® 7 BA 01 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 7 BA 01 is used for film coextrusion and lamination where sealab..
Melt Index of Compound 1.0 - 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 - 1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Arkema Group OREVAC® C306 Maleic Anhydride Modified Linear Low Density Polyethylene
OREVAC C306 is anhydride modified LLDPE. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. It has been designed..