Polymer Property : Melt Index of Compound = 1.4 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
carrier resin value; ASTM D-1238
Chevron Phillips MarFlex® ER3341 Polyethylene; Masterbatch  (discontinued **)
Metallocene polyethylene antiblock masterbatch. This antiblock concentrate with its mLLDPE carrier is tailored for use with mPACT™ resins in blown film applications that require: Reduced COFMinim..
Melt Index of Compound 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
carrier resin value; ASTM D-1238
Chevron Phillips MarFlex® ER3343 Polyethylene; Masterbatch  (discontinued **)
Metallocene polyethylene slip masterbatch. This erucamide slip concentrate with its mLLDPE carrier is tailored for use with mPact™ resins in blown film applications that require: Reduced COFExcel..
Melt Index of Compound 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
carrier resin value; ASTM D-1238
Chevron Phillips MarFlex® ER3344 Polyethylene; Masterbatch  (discontinued **)
Metallocene polyethylene antiblock masterbatch. This erucamide slip and antiblock concentrate with its mLLDPE carrier is tailored for use with mPACT™ resins in blown film applications that require..
Melt Index of Compound 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Chevron Phillips MarFlex® 7114 Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L..
Melt Index of Compound 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Chevron Phillips Marlex® C101 Polyethylene; Enhanced
Metallocene linear low density polyethylene. This linear low density, hexene copolymer is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typi..