Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Lendell Parapet EH-1000 PMMA, Extrusion |
|||
Melt Index of Compound | 1.2 g/10 min | 1.2 g/10 min | |
Lushan LR-1D Halogen-Free Flame-Retardant Compatibilizer Halogen-free flame retardant compatibilizer Lushan series for cables and wires are developed by several doctors and maters from Lushan’s R&D Center, and combined ten years’ modified polyol.. |
|||
Melt Index of Compound | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® ENR 7467.00 Ethylene-Butene Copolymer Description: ENR 7467.00 is a high performance ethylene-butene copolymer, offering superior impact properties for more demanding TPO applications. The polymer has very low crystallinity and is avail.. |
|||
Melt Index of Compound | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group OREVAC® 18302N Maleic Anhydride Modified Linear Low Density Polyethylene OREVAC® 18365 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Melt Index of Compound | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Arkema Group OREVAC® 18319 Grafted Maleic Anhydride Polyethylene OREVAC 18319 is a maleic anhydride grafted polyethylene used in the manufacturing of multi-layer aluminium panels. OREVAC 18319 is mainly used in aluminium panels to have good adhesion performances .. |