Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.60 g/10 min | 0.60 g/10 min | ASTM D1238 |
Polymer Industries Densetec PP Homopolymer Sheet Polymer Industries’ Densetec Homopolymer Polypropylene exhibits the properties of high corrosion resistance, high temperature resistance, and great tensile strength. It maintains its stiffness at e.. |
|||
Melt Index of Compound | 0.60 g/10 min | 0.60 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.60 g/10 min | 0.60 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.60 g/10 min | 0.60 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.60 g/10 min | 0.60 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow FINGERPRINT™ DFDA-7510 NT Linear Low Density Polyethylene Resin FINGERPRINT™ DFDA-7510 NT resin is produced using UNIPOL™ process technology. It is intended for use in micro irrigation tube, durable hose and tube, profile extrusion, and injection molded fitti.. |
|||
Melt Index of Compound | 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-7441 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in hose and tube applications. It also has utility in gasketing, spiral wound hose, and corrugated hose .. |
|||
Melt Index of Compound | 0.60 g/10 min | 0.60 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.60 g/10 min | 0.60 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |