Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.12 - 0.16 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.12 - 0.16 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TU 3001 LDPE - Agricultural Film The Trithene TU 3001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical properties, good processability and bu.. |