Physical Properties Metric English Comments
Linear Mold Shrinkage 0.020 cm/cm

@Thickness 6.35 mm
0.020 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.020 - 0.025 cm/cm

@Thickness 6.35 mm
0.020 - 0.025 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.020 - 0.024 cm/cm

@Thickness 6.35 mm
0.020 - 0.024 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.020 - 0.024 cm/cm

@Thickness 6.35 mm
0.020 - 0.024 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.020 - 0.024 cm/cm

@Thickness 6.35 mm
0.020 - 0.024 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.020 - 0.024 cm/cm

@Thickness 6.35 mm
0.020 - 0.024 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.020 cm/cm

@Thickness 2.00 mm
0.020 in/in

@Thickness 0.0787 in
Parallel; ISO 294-4
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer
Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a..
Linear Mold Shrinkage 0.020 cm/cm

@Thickness 2.00 mm
0.020 in/in

@Thickness 0.0787 in
Parallel; ISO 294-4
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer
Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic..
Linear Mold Shrinkage 0.020 cm/cm

@Thickness 2.00 mm
0.020 in/in

@Thickness 0.0787 in
Normal; ISO 294-4
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer
Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro..