Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.020 cm/cm @Thickness 6.35 mm |
0.020 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.020 - 0.025 cm/cm @Thickness 6.35 mm |
0.020 - 0.025 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.020 - 0.024 cm/cm @Thickness 6.35 mm |
0.020 - 0.024 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.020 - 0.024 cm/cm @Thickness 6.35 mm |
0.020 - 0.024 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.020 - 0.024 cm/cm @Thickness 6.35 mm |
0.020 - 0.024 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.020 - 0.024 cm/cm @Thickness 6.35 mm |
0.020 - 0.024 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
Parallel; ISO 294-4 |
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a.. |
|||
Linear Mold Shrinkage | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
Parallel; ISO 294-4 |
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |
|||
Linear Mold Shrinkage | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
Normal; ISO 294-4 |
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro.. |