Polymer Property : Linear Mold Shrinkage = 0.015 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.012 - 0.015 cm/cm

@Thickness 3.20 mm
0.012 - 0.015 in/in

@Thickness 0.126 in
Transverse, 24h; ASTM D955
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer  (Unverified Data**)
Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide..
Linear Mold Shrinkage 0.010 - 0.015 cm/cm

@Thickness 2.50 - 5.00 mm
0.010 - 0.015 in/in

@Thickness 0.0984 - 0.197 in
ASTM D955
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.