Linear Mold Shrinkage 0.013 cm/cm

@Thickness 3.17 mm
0.013 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.013 - 0.017 cm/cm

@Thickness 3.17 mm
0.013 - 0.017 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.013 - 0.017 cm/cm

@Thickness 3.17 mm
0.013 - 0.017 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.013 - 0.016 cm/cm

@Thickness 6.35 mm
0.013 - 0.016 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 6.35 mm
0.013 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 3.20 mm
0.013 in/in

@Thickness 0.126 in
Transverse
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT
Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide..