Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.012 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.012 - 0.015 cm/cm

@Thickness 3.20 mm
0.012 - 0.015 in/in

@Thickness 0.126 in
Transverse, 24h; ASTM D955
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer  (Unverified Data**)
Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide..
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 6.35 mm
0.012 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/TC/20/FD Polypropylene Homopolymer, 20% Talc Filled, FDA compliant
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.012 - 0.014 cm/cm

@Thickness 3.17 mm
0.012 - 0.014 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 6.35 mm
0.012 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-61/TC/20 Polypropylene Copolymer, 20% Talc
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 6.35 mm
0.012 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.012 - 0.014 cm/cm

@Thickness 3.17 mm
0.012 - 0.014 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.012 - 0.021 cm/cm

@Thickness 1.60 mm
0.012 - 0.021 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax CCP PBT 1100-220S
Product Description: PBT unreinforced and impact-modified injection molding grade. Characteristics:Low warp age, high toughness and excellent dimensional stabilityExcellent glossy surface and less-g..
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 6.35 mm
0.012 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-15/T/10/20 Polypropylene Homopolymer, 22% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 3.17 mm
0.012 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.012 - 0.018 cm/cm

@Thickness 1.60 mm
0.012 - 0.018 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 3020-104 15% Glass Fiber Filled
Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.012 - 0.016 cm/cm

@Thickness 3.20 mm
0.012 - 0.016 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 341 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.012 - 0.014 cm/cm

@Thickness 3.00 mm
0.012 - 0.014 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.012 - 0.016 cm/cm

@Thickness 3.20 mm
0.012 - 0.016 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 341 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.012 - 0.016 cm/cm

@Thickness 3.20 mm
0.012 - 0.016 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 341 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.012 - 0.016 cm/cm

@Thickness 3.20 mm
0.012 - 0.016 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 341 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.012 - 0.016 cm/cm

@Thickness 3.20 mm
0.012 - 0.016 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 341 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.012 - 0.014 cm/cm

@Thickness 3.00 mm
0.012 - 0.014 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.012 cm/cm

@Temperature 240 °C
0.012 in/in

@Temperature 464 °F
ASTM D3392
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Linear Mold Shrinkage 0.012 cm/cm

@Temperature 240 °C
0.012 in/in

@Temperature 464 °F
ASTM D3392
DuPont™ Nomex® Type 993, 95 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Copyright © lookpolymers.com All Rights Reserved