Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0080 cm/cm @Thickness 3.20 mm |
0.0080 in/in @Thickness 0.126 in |
Transverse; DAM |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.0080 cm/cm @Thickness 6.40 mm |
0.0080 in/in @Thickness 0.252 in |
Transverse; DAM |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 3030-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.016 cm/cm @Thickness 1.60 mm |
0.0080 - 0.016 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 2100-104B Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 3030-104 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 389 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 389 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0080 cm/cm @Temperature 105 °C |
0.0080 in/in @Temperature 221 °F |
ASTM D3392 |
DuPont™ Nomex® Type 993, 95 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Linear Mold Shrinkage | 0.0080 cm/cm @Thickness 1.60 mm |
0.0080 in/in @Thickness 0.0630 in |
Flow; DAM |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Linear Mold Shrinkage | 0.0080 cm/cm @Thickness 1.60 mm |
0.0080 in/in @Thickness 0.0630 in |
Transverse; DAM |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.013 cm/cm @Thickness 3.00 mm |
0.0080 - 0.013 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PBT 5630-200C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |