Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-60/10/E Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-69/10/E High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0060 - 0.0070 cm/cm @Thickness 6.35 mm |
0.0060 - 0.0070 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-60/TC/40/OP WT2595 Polypropylene Homopolymer, 40% Talc Filled, high opacity Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm @Thickness 3.00 mm |
0.0060 - 0.0080 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm @Thickness 1.00 mm |
0.0060 - 0.0080 in/in @Thickness 0.0394 in |
DAM |
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (Conditioned) Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm @Thickness 1.00 mm |
0.0060 - 0.0080 in/in @Thickness 0.0394 in |
|
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM) Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.0060 - 0.012 cm/cm @Thickness 1.00 mm |
0.0060 - 0.012 in/in @Thickness 0.0394 in |
DAM |
Toyobo T-661 Nylon 66, Standard Grade (Conditioned) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |