Polymer Property : Linear Mold Shrinkage = 0.0015 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..