Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | STN EN ISO 294-4 |
Plastcom PLASTAMID® 66 BT B 27 TS PA66 heat stabilized Basic type PA66 for injection molding, heat stabilized, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - elec.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Plastcom SLOVALEN PH 99 GB 20 PP, 20% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE70-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
Mold Temp 80°C; Melt Temp 280°C; 600 bar; ISO 294-4 |
Lanxess Durethan® A 30 H3.0 000000 Nylon 66 PA 66, non reinforced, injection molding, heat-ageing stabilized |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 150x105x3, 260°C / MT 80°C; 500 bar; acc. ISO 2577 |
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.021 cm/cm | 0.019 - 0.021 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA) Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 216 PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 217 PA66, DRY Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® 2710IR PA66, DRY Description: TECHNYL® 2710 IR is an unfilled polyamide 6.6, impact modified, for injection molding. The product is available in natural color, and in colors on request.Benefits: This product, use.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
Teknor Apex Telcar® TL-1137 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1606-N Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® CE2055 BK580 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin CE2055 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performanc.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers with very low VOC emissi.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX SG 40 A.01 black TPE-S, Shore A40, black TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.030 cm/cm @Time 86400 sec |
0.019 - 0.030 in/in @Time 24.0 hour |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 60x60x2mm; ISO 294 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.021 cm/cm @Time 86400 sec |
0.019 - 0.021 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf P1000EI3 PA 6 (Asia Pacific) High Impact Nylon 6 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® CE2055 BK580 PBT
(Unverified Data**) Crastin® CE2055 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information p.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |