Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0162 cm/cm | 0.0162 in/in | |
Plastcom SLOVAMID 6 GF 20 PA6, 20% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Linear Mold Shrinkage, Transverse | 0.0162 cm/cm | 0.0162 in/in | |
Plastcom SLOVAMID 6 GB 20 PA6 reinforced with 20% glass beads Features: Nearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical proper.. |