Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0131 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0131 cm/cm
0.0131 in/in
Plastcom SLOVALEN PC 71 GF 10 PP, 10% glass fibre
FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass fibre and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s..
Linear Mold Shrinkage, Transverse 0.0131 cm/cm
0.0131 in/in
Plastcom SLOVALEN PQ 91T 5 PP, 5% mineral filling
FeaturesModified PP for injection moulding with the content of 5 % mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene..
Linear Mold Shrinkage, Transverse 0.0131 cm/cm
0.0131 in/in
Plastcom SLOVALEN PH 59 T 40 LW 031 PP, 40% mineral filling, laser label
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc.Contains modificator for laser labeling of finisched parts. /LASER NdIAG..
Copyright © lookpolymers.com All Rights Reserved