Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.012 - 0.013 cm/cm | 0.012 - 0.013 in/in | ASTM D955 |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO 294-4 |
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | ASTM D955 |
PolyOne Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm @Thickness 3.18 mm |
0.011 - 0.013 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® PS-30CF/000 HF UV BLACK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Later 4 G/30 PBT, 30% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Transverse | 0.0095 - 0.013 cm/cm | 0.0095 - 0.013 in/in | |
LATI Latilub 62-15ST PA6 Self-lubricating product based on Polyamide 6 (PA6). Silicone / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm @Thickness 0.750 - 2.30 mm |
0.0090 - 0.013 in/in @Thickness 0.0295 - 0.0906 in |
SABIC Method |
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.013 cm/cm @Thickness 3.20 mm |
0.0080 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQNH4550 PBT Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% .. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.013 cm/cm @Time 86400 sec |
0.0060 - 0.013 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp WC003P Polyester Elastomer LNP* Thermocomp* WC003P is a compound based on Polyester resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.013 cm/cm @Thickness 3.20 mm |
0.0080 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA (Asia Pacific) High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific) High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ISO DIS 294-4 |
Wellman EcoLon® MR1660-BK 40% Mineral Reinforced Post Consumer Compound Nylon 66 Description: Mineral Reinforced Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF33-66/6 XE-BK167A 33% Glass Filled, Color Matched Ebony Nylon 66/6 Description: Glass Filled, Color Matched Ebony Nylon 66/6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | DIS 294-4 |
Wellman Wellamid® GF33A099-HRBK Nylon 66, 33% Glass Fiber Reinforced, Hydrolysis Resistant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | DIS 294-4 |
Wellman Wellamid® GS1861-N1(PTFE) Nylon 66, 35% Glass Sphere Reinforced, Enhanced Lubrication All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | DIS 294-4 |
Wellman Wellamid® MR340 42H-NBK1 Nylon 6, 34% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | DIS 294-4 |
Wellman Wellamid® MRGF1647-BK1 Nylon 66, 40% Mineral/Glass Fiber Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | DIS 294-4 |
Wellman Wellamid® MRGF25/25 22H-NBK1 Nylon 66, 25% Mineral and 25% Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1599-BK Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1599-GY Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Asahi Kasei Method |
Asahi Kasei Tenac® GA510 Homopolymer Acetal Resin 10% Glass fiber filled grade with high stiffness and superior dimensional stability.Information provided by Asahi Kasei Corporation. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | ASTM D955 |
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Latilub 67-10STE21 G/20 PA66, 20% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66), impact modified. Silicone / PTFE. Toughened. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |