Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0120 cm/cm | 0.00700 - 0.0120 in/in | Average value: 0.00995 cm/cm Grade Count:4 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0120 cm/cm | 0.00200 - 0.0120 in/in | Average value: 0.00545 cm/cm Grade Count:34 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Linear Mold Shrinkage, Transverse | 0.00300 - 0.0120 cm/cm | 0.00300 - 0.0120 in/in | Average value: 0.00596 cm/cm Grade Count:27 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Linear Mold Shrinkage, Transverse | 0.00150 - 0.0120 cm/cm | 0.00150 - 0.0120 in/in | Average value: 0.00781 cm/cm Grade Count:53 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00480 - 0.0120 cm/cm | 0.00480 - 0.0120 in/in | Average value: 0.00765 cm/cm Grade Count:11 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0120 cm/cm | 0.00800 - 0.0120 in/in | Average value: 0.0104 cm/cm Grade Count:5 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0120 cm/cm | 0.00700 - 0.0120 in/in | Average value: 0.00888 cm/cm Grade Count:8 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0120 cm/cm | 0.00100 - 0.0120 in/in | Average value: 0.00697 cm/cm Grade Count:37 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0120 cm/cm | 0.00100 - 0.0120 in/in | Average value: 0.00879 cm/cm Grade Count:13 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |