Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0091 cm/cm | 0.0091 in/in | |
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre FeaturesChemically reinforced with 13% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Linear Mold Shrinkage, Transverse | 0.0091 cm/cm | 0.0091 in/in | ISO 294-4, 2577 |
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules |
|||
Linear Mold Shrinkage, Transverse | 0.0091 cm/cm | 0.0091 in/in | ISO 294-4, 2577 |
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Linear Mold Shrinkage, Transverse | 0.0091 - 0.0093 cm/cm @Time 86400 sec |
0.0091 - 0.0093 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Asia Pacific) LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N.. |
|||
Linear Mold Shrinkage, Transverse | 0.0091 - 0.0093 cm/cm @Time 86400 sec |
0.0091 - 0.0093 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N.. |
|||
Linear Mold Shrinkage, Transverse | 0.0091 cm/cm | 0.0091 in/in | 60x60x2 mm; ISO 294 |
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 20% of glass fibers for industrial parts with high dimensional stab.. |