Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | |
Plastcom SLOVALEN PH 59 GF 30 PP, 30% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suita.. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | |
Plastcom SLOVAMID 66/6 T 30 TS PA66/6, 30% mineral filling FeaturesPA 66/PA 6 alloy with the content of 30 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, autom.. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | |
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | 60x60x2; 290°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® AKV 30 G HR DUS023 900116 Nylon 66, 30% Glass Fiber PA 66, 30% glass fiber, injection molding, improved flowability, hydrolysis stabilized, improved surface finish, GIT/WITInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, good heat-ageing resistance and hydrolysis resistance, good flowability (Easy Flow) |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP AKV 30 X HR EF 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis and good heat-ageing resistance, good flowability (Easy Flow) |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance, and hydrolysis resistanceApplication Examples: coolant manifolds |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | ASTM D955 |
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount .. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | ISO 294-4 |
DSM Akulon® K222-KMV5 /A PA6-MD25 FR(30) 25% Mineral Reinforced, Flame Retardant (Halogen free), Color Stabilized |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | ISO 2577 |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | ISO 2577 |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | Sheet |
BASF Ultradur S 4090 G4 20% Glass Filled PBT Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio.. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | ISO Data |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm | 0.0082 in/in | 60x60x2 mm; ISO 294 |
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab.. |