Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0077 cm/cm | 0.0077 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Linear Mold Shrinkage, Transverse | 0.0077 cm/cm | 0.0077 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP 2802/30 000000 Nylon 66, 30% Glass Fiber PA 66 injection molding grade, 30% glass fibers, UL 94V-2 at 0.75 mm , GWFI:960°C at 0.75 mm, GWIT: 775°C at 0,75 mm, halogen-freeApplication Examples: mixer insert for blenders, washing machi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0077 cm/cm | 0.0077 in/in | ASTM D955 |
Teknor Apex Sinpolene GPP5620 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 20% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Linear Mold Shrinkage, Transverse | 0.0077 cm/cm | 0.0077 in/in | Sim. To ISO 294 |
DSM Akulon® Ultraflow K-FKGS6 /B PA6-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
Linear Mold Shrinkage, Transverse | 0.0077 cm/cm | 0.0077 in/in | 60x60x2mm; ISO 294 |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
Linear Mold Shrinkage, Transverse | 0.0077 cm/cm | 0.0077 in/in | ISO 2577 |
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl.. |
|||
Linear Mold Shrinkage, Transverse | 0.0077 cm/cm | 0.0077 in/in | ISO 294 |
BASF Ultrason S 6010 PSU Ultrason S 6010 is an unreinforced, high molecular weight injection-molding and extrusion grade with excellent chemical resistance (stress crack resistance) and good solubility in typical solvents (.. |