Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0073 cm/cm | 0.0073 in/in | |
Plastcom SLOVAMID 66 CF 40 PA66, 40% carbon fibre FeaturesChemically reinforced with 40% carbon fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. .. |
|||
Linear Mold Shrinkage, Transverse | 0.0073 cm/cm | 0.0073 in/in | STN 64 0808 |
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Linear Mold Shrinkage, Transverse | 0.0073 cm/cm @Time 86400 sec |
0.0073 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Linear Mold Shrinkage, Transverse | 0.0073 cm/cm @Time 86400 sec |
0.0073 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Linear Mold Shrinkage, Transverse | 0.0073 cm/cm @Time 86400 sec |
0.0073 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Linear Mold Shrinkage, Transverse | 0.0073 cm/cm @Time 86400 sec |
0.0073 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon DS0029 PC LNP STAT-KON* DS0029 is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for t.. |
|||
Linear Mold Shrinkage, Transverse | 0.0073 cm/cm @Time 86400 sec |
0.0073 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON MVL36SX0 PP (Europe-Africa-Middle East) LNP* VERTON* MVL36SX0 is a compound based on PP resin containing Long Glass Fiber and PTFE. Added features include: Chemically coupled, Heat Stabilized, Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0073 cm/cm | 0.0073 in/in | ISO 2577, 294-4 |
BASF Ultrason® S 3010 MR UN PSU Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1.. |